UNS S32750

 

page-800-800
page-800-800
page-800-800
page-800-800
page-600-600

 

Details

 

Lork Group high-quality UNS S32750 is a duplex stainless steel has very good resistance to localized corrosion and stress corrosion cracking in combination with high mechanical strength.

 

Products Description

 

Lork Group high-quality UNS S32750 (1.4410 /F53) is a duplex stainless steel designed for service in aggressive chloride-containing environments. It has very good resistance to localized corrosion and stress corrosion cracking in combination with high mechanical strength. It is widely used in oil & gas, hydropower, pressure vessels, pulp & paper, structural components and chemical tankers.

UNS S32750 high mechanical strength (typically up to 570 MPa yield strength) and good ductility with outstanding corrosion resistance in marine environments. The alloy is supplied with a PREN (Pitting Resistance Equivalent) at >=40.0 which guarantees high resistance to pitting corrosion. In addition, the steel offers high resistance to crevice corrosion and stress corrosion cracking. Ambient and sub-zero (down to minus 50°C) notch ductility is good.

 

Product Form

 

Round bar

Plate

Sheet

Round tube

 

UNS S32750 Chemical Composition

 

Element

Content (%)

Cr

24 – 26

Ni

6 – 8

Mo

3 – 5

Mn

1.20 max

Si

0.80 max

Cu

0.50 max

N

0.24 – 0.32

P

0.035 max

C

0.030 max

S

0.020 max

Fe

Balance

 

UNS S32750 Physical Properties

 

Properties

Metric

Imperial

Density

7.8 g/cm3

0.281 lb/in3

Melting point

1350°C

2460°F

 

UNS S32750 Applications

 

  • Power
  • Marine
  • Chemical
  • Pulp and paper
  • Petrochemical
  • Water desalinization
  • Oil and gas production
  • Pumps, valves, chokes
  • Pipework/flanges
  • Connectors
  • Manifolds

 

Send Inquiry Now