Invar 36 Nickel Alloy Strip (UNS K93603, ASTM F1684)

Invar 36 Nickel Alloy Strip (UNS K93603, ASTM F1684)

Invar 36 is a low-expansion Ni-Fe alloy with a linear thermal expansion coefficient of approximately 1.2 × 10⁻⁶/°C in the range of -250°C to +200°C.
Send Inquiry

Products Description

 

Invar 36 strip is primarily supplied in thicknesses ranging from 0.2 mm to 2.0 mm and widths from 10 mm to 200 mm (custom dimensions are available); it can be provided either in cut-to-length pieces or in coils. Prices generally range from $60 to $80 per kilogram, depending on the supply condition and order quantity; please contact us to confirm the current price.

 

Invar 36 (also known as Invar alloy; corresponding to the Chinese grade 4J36) is an iron-nickel low-expansion precision alloy with a nickel content of approximately 36%. Its most distinctive characteristic is an extremely low coefficient of thermal expansion over a wide temperature range: between -60°C and +200°C, the average linear expansion coefficient is controlled within the range of 1.2×10⁻⁶/°C to 1.5×10⁻⁶/°C-roughly one-tenth that of ordinary carbon steel or austenitic stainless steel.

 

This "zero-expansion" property stems from the specific ratio of nickel (approximately 36%) to iron. At temperatures below the Curie point (approximately 230°C), the alloy is ferromagnetic; the magnetostrictive effect counteracts the thermal expansion caused by lattice thermal vibrations, resulting in virtually constant dimensions at the macroscopic level. Invar 36 strip offers a balance of moderate strength, toughness, and good workability, allowing it to be processed-via cold rolling, stamping, bending, and other methods-into thin strips and components with complex shapes.

 

Implementation Standard

Standard designation
ASTM F1684
ASTM B753
4J36( YB/T 5241 )
W.Nr. 1.3912
Standard Title Standards specifically developed for electronic components and microelectronic packaging. General technical specifications for low-expansion alloy strips, sheets, and foils Technical Specifications for General-Purpose Low-Expansion Alloys Nickel-iron alloy standard
Applicable Scenarios Semiconductor lead frames, optical communication modules, precision photomask frames, etc. General Procurement and Acceptance of Precision Alloy Strip. Traditional industrial sectors such as precision instruments, standard measuring tools, waveguides, and the inner walls of LNG storage tanks. Applications of Low-Expansion Alloys in the European Market

 

Selection Note: For electronic-grade applications such as semiconductor equipment or optical communication modules, the use of ASTM F1684 Grade 2 material is recommended. If design specifications are based on the thermal expansion coefficient requirement of ≤1.2×10⁻⁶/°C from the YB/T 5241 standard, the equivalent expansion coefficient requirement must be stipulated in the contract when purchasing ASTM-standard materials.

 

Precautions for Processing and Use 

 

Heat Treatment Sensitivity: The low-expansion characteristics of Invar 36 depend on proper heat treatment. Annealing temperatures exceeding 850°C cause rapid grain growth, leading to an increased coefficient of thermal expansion. Stress-relief annealing is required after cold working; otherwise, residual stresses may cause dimensional drift during service.

Machining Recommendations: Invar 36 produces sticky chips and is prone to built-up edge formation. Carbide tools are recommended, with cutting speeds maintained between 40 and 60 m/min and the use of ample coolant/lubricant.

Corrosion Protection: Invar 36 is susceptible to rusting in humid air; surface protection (such as nickel plating, chrome plating, or coating) is recommended for long-term use or outdoor applications.

Curie Temperature Limitation: Above approximately 230°C, the low-expansion properties are lost, and the coefficient of thermal expansion increases significantly to over 10 × 10⁻⁶/°C. Operating temperatures must remain below this threshold.

For more information, please contact:

Email: claire@lorkgroup.com
WhatsApp: +86 199 3707 5488

Invar 36 strip

 

chemical composition

 

Element content(%)

Ni

35.00–37.00

Fe

rest

C

max0.05

Mn

0.20–0.60

Si

max0.30

P

max0.02

S

max0.02

Cr

max0.50

Co

max1.00

*Data based on the ASTM F1684 standard specification.

 

Mechanical properties (room temperature, annealed)

 

Metric Invar 36
Tensile Strength 490 MPa
Yield Strength 0.2% 240 MPa
Elongation 42%

 

Lork Group
Marketing Operations Department

Email: claire@lorkgroup.com
WhatsApp: +86 199 3707 5488

Hot Tags: Invar 36, Alloy 36, UNS K93601, W.-Nr. 1.3912, ASTM F1684, ASTM B753, 4J36, Nilo36, Pernifer 36, low expansion alloy strip, invariable alloy, precision alloy strip, cryogenic alloy strip, aerospace alloy strip

Send Inquiry