Nimonic 115

Our Lork Group supplies Nimonic 115 bars and plates. For more details, please click the link in the image below. We also welcome inquiries about other profiles.

Nimonic 115 Nickel Alloy Bar
page-600-600
Nimonic 115 Alloy Sheet
page-600-600
page-600-600

 

Details

 

Lork Group's high-quality Nimonic 115 is a nickel-chromium-cobalt-molybdenum alloy that can be precipitation-hardened. It is suitable for oxidation resistance and high-temperature strength.

Need a quote or size information? Feel free to contact us!

📧 layla@lorkgroup.com | 📞 +86 199 3707 5488

 

Products Description

 

Lork Group's high-quality Nimonic 115 is a nickel-chromium-cobalt-molybdenum alloy that can be precipitation-hardened. It is suitable for oxidation resistance and high-temperature strength. Application: It was developed as a creep-resisting alloy for service at temperatures up to about 1010°C, as turbine blades for aircraft gas turbines.

Offering superior oxidation resistance and high-temperature strength, the original intended application for this product was in the production of gas turbine blades. Heat treatment of the product is by solution treatment and then ageing.

 

Product Form

 

Plate,Sheet & Strip: BS HR4

 

Nimonic 115 Chemical Composition

 

Element

Content (%)

Ni

54

Cr

14.0-16.0

Co

13.0-15.5

Al

4.50-5.50

Mo

3.0-5.0

Ti

3.50-4.50

Fe

1.0

Mn

1.0

Si

1.0

Cu

0.20

Zr

0.15

C

0.12-0.20

S

0.015

B

0.010-0.025

 

Nimonic 115 Property

 

Properties

Metric

Imperial

Tensile strength

1300 MPa

189000 psi

Yield strength

850 MPa

123000 psi

Elongation at break

25.00%

25.00

 

Nimonic 115 Application

 

Nimonic 115 is suitable for use in high-temperature components in gas turbine applications.

 

Send Inquiry Now