Lork Group high-quality Invar 36 (UNS K93603) is a nickel-iron, low expansion alloy that contains 36% nickel ,This nickel iron alloy is tough, versatile and retains good strength at cryogenic temperatures.

 

Products Description

 

Lork Group high-quality Invar 36 (UNS K93603) is a nickel-iron, low expansion alloy that contains 36% nickel and possesses a rate of thermal expansion approximately one-tenth that of carbon steel.

Invar 36 maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coefficient of expansion from cryogenic temperatures to about 500°F. This nickel iron alloy is tough, versatile and retains good strength at cryogenic temperatures.

Invar 36 (also known as Nilo, Nilvar, Permalloy D, FeNi36, and 64FeNi) is an nickel-iron alloy notable for its extremely low thermal expansion. Primary uses for Invar include laser and cryogenic components, tooling, dies, and any other application requiring high dimensional stability.

 

Product Form

 

Sheet/Plate/Strip: ASTM B388, ASTM B753, DIN 1715, ASTM F1684

Round Bar: ASTM F1684

 

Invar 36 Chemical Composition

 

Element

Content

C

0.15 max

Mn

0.6 max

P

0.006 max

S

0.004 max

Si

0.4 max

Cr

0.25 max

Ni

36.0

Co

0.5 max

Fe

balance

 

Invar 36 Property

 

Temperature

Yield Strength

Tensile Strength

Elongation

Reduction

°C

°F

MPa

Psi

MPa

Psi

2" %

%

20

68

240

35.0

490

71.0

42

70

 

Invar 36 Application

 

  • Tooling and Dies for Aerospace Composite
  • ToolingThermoset Epoxy Systems
  • Resin Transfer Molded Tools
  • Cryogenic Components and Piping
  • Laser Components
  • Liquified Natural Gas (LNG)Marine fixtures and fasteners Production and Storage Equipment
  • LNG Tanker Membranes
  • Marine Components
  • Wind Turbines

 