Incoloy 330

 

page-600-600
page-600-600
Incoloy 330 Nickel Alloy Plate
page-600-600
page-600-600

Details

 

Lork Group high-quality Incoloy 330 (UNS N08330; W. Nr. 1.4886) is an austenitic alloy with good high-temperature strength and corrosion resistance. It has a solid solution composition and is not hardenable by heat treatment.

 

Products Description

 

Lork Group high-quality Incoloy 330 (UNS N08330; W. Nr. 1.4886) is an austenitic alloy with good high-temperature strength and corrosion resistance. It has a solid solution composition and is not hardenable by heat treatment.

 

Its high nickel and chromium provide good resistance to oxidation and carburization. Its oxidation resistance is enhanced by the silicon content. The alloy's strength and oxidation resistance at elevated temperatures make it a useful material for industrial heating furnaces; for muffles, retorts, conveyor systems, baskets and boxes, and various fixtures.

 

Incoloy 330 is also known for its good fabricability, including excellent weldability and formability. This allows it to be easily shaped and joined, making it a versatile material for a variety of manufacturing processes.

 

Product Form

 

Sheet/Plate/Strip: AMS 5592, ASTM B536

Bars/Wire/Forgings/Flash welded rings: AMS 5716

Bar: ASTM B511

Seamless Pipe: ASTM B535

Pipe/Tube: ASTM B546

Welded Pipe: ASTM B710

 

Chemical Composition

 

Element

Content (%)

Iron, Fe

43

Nickel, Ni

34-37

Chromium, Cr

17-20

Manganese, Mn

≤2

Others

Remainder

 

Physical Properties

 

Properties

Metric

Imperial

Density

8.08 gm/cm3

0.292 lb/in3

 

Mechanical Properties

 

Properties

Metric

Imperial

Tensile strength(annealed)

600 MPa

87 ksi

Yield strength(annealed)

280 MPa

40.6 ksi

Elongation at Break

45%

45%

 

Applications

 

  • Heat treating equipment
  • Furnace muffles
  • Retorts
  • Conveyor systems
  • Magnetostrictive transducers
  • Mechanical supports
  • Transistor housings
  • Battery cases
  • Lead wires
  • Anodes and grids of electronic valves.

 

Send Inquiry Now