Lork Group high-quality AISI 304 (1.4301/X5CrNi18-10) is the standard material of austenitic chromium-nickel steels. Good corrosion resistance in natural environmental media. Not suitable for use in chlorine and salt concentrations.

 

Products Description

 

Lork Group high-quality AISI 304 (1.4301/X5CrNi18-10) is the standard material of austenitic chromium-nickel steels. Good corrosion resistance in natural environmental media. Not suitable for use in chlorine and salt concentrations. Risk of intergranular corrosion at high temperatures, for example during welding.

The materials AISI 304L and AISI 321 have comparable chemical composition and properties.

Materials in a higher nickel-alloyed version are recommended with continually increasing demands on formability.

 

Product Form & Standard

 

Sheet / strip 125ksi AMS 5501
Sheet /strip (ann) AMS 5501
Sheet / strip (ann) AMS 5513
Seamless tube AMS 5560
1/4Hd Seamless/welded AMS 5560
1/8Hd Seamless/welded AMS 5564
Welded tube AMS 5565
Seamless/welded tube AMS 5566, AMS 5567, AMS 5569
Welded tube AMS 5575
304 Bar / Forgings AMS 5639

 

AISI 304 Chemical composition

 

Element

Content (%)

C

0.08 max

Si

1.00 max

Mn

2.0 max

P+S

0.040 P 0.03 S

Cr

18.0 - 20.0

Ni

8.0 - 10.5

Fe

Bal

Mo

0.75 max

Cu

0.75 max

 

AISI 304 Mechanical Properties

 

Specification

Tensile Strength (ksi)

Yield Strength (ksi)

Elongation (%)

Reduction of Area

Hardness HB

Sheet (Annealed) AMS 5511

100 max

-

40

-

-

Sheet (Annealed) AMS 5513

75 min

30

40

-

202

Bar (Sol Treated) 304 - AMS 5639

75

30

40

50

 

 